Nd:Ce:Technical zviratidzo zveYAG laser crystal tsvimbo | |
Doping concentration | Nd:0.1~1.4at%,Ce:0.05~0.1at% |
Crystal orientation | <111>+50 |
Transmission wavefront distortion | s0.1A/inch |
Extinction ratio | ≥25dB |
Saizi yechigadzirwa | Diameter≤50mm, Length≤150 mmSlats uye madhisiki anogona kugadzirwa maererano nezvinodiwa nemutengi. |
Dimensional kushivirira | Diameter:+0.00/-0.05mm,Kureba:±0.5mm |
Cylindrical surface processing | Kukuya zvakanaka, kukwenenzvera, kupinza |
Kugumisa kufanana kwechiso | ≤ 10” |
Iyo perpendicularity yemagumo yakatarisana neiyo tsvimbo axis | ≤ 5' |
Kupedza chiso flatness | 入/10 @632.8nm |
Surface quality | 10-5 (MIL-0-13830A) |
Chamfer | 0.15+0.05mm |
Coating | S1/S2:R@1064nms0.2% |
S1:R@1064nm≤0.2%,S2:R@1064=20+3% | |
S1:R@1064nm≤0.2%,S2:R@1064nmz99.8% | |
Mamwe mafirimu masisitimu anogona kugadzirwa. | |
Iyo laser kukuvara chikumbaridzo cheiyo firimu layer | ≥500MW/cm2 |
Laser wavelength | 1064nm |
Diode pumped absorption wavelength | 808nm |
Refractive index | 1.8197@1064nm |
special | Surface metallization |
Pedzisa kumeso wedge angle, concave/convex surface, nezvimwe. |